Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 19.6 kV/mm @Thickness 3.17 mm |
498 kV/in @Thickness 0.125 in |
|
Advanced Elastomer Systems Santoprene® 153-38 Thermoplastic Rubber
(discontinued **) A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be pr.. |
|||
Dielectric Strength | 19.6 kV/mm @Thickness 3.17 mm |
498 kV/in @Thickness 0.125 in |
|
Advanced Elastomer Systems Santoprene® 221-73 W175 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic UV grade elastomer designed for thin wall extrusion applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and c.. |
|||
Dielectric Strength | 19.6 kV/mm @Thickness 3.17 mm |
498 kV/in @Thickness 0.125 in |
|
Advanced Elastomer Systems Santoprene® 251-80 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Dielectric Strength | 19.6 kV/mm @Thickness 3.17 mm |
498 kV/in @Thickness 0.125 in |
|
Advanced Elastomer Systems Santoprene® 253-36 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Dielectric Strength | 19.6 kV/mm @Thickness 3.17 mm |
498 kV/in @Thickness 0.125 in |
|
Advanced Elastomer Systems Santoprene® 253-50 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Dielectric Strength | 19.6 kV/mm | 498 kV/in | Perpendicular S/T in Air; ASTM D-149 |
Glastic SG-200 Industrial Lift Magnet Glastic Grade SG-200 high-strength and high-temperature laminates offer temperature ratings of up to 210°C. SG-200 is ideal for a wide variety of product applications requiring high-temperature .. |
|||
Dielectric Strength | 19.6 kV/mm | 498 kV/in | Perpendicular in Air; ASTM D-149 |
Glastic T-160 Fiberglass-Reinforced Polyester Laminate Grade T-160 is a new, high-strength, heat-resistant laminate. This highly creep-resistant material is excellent for applications where electrically insulating materials are subject to physical load.. |
|||
Dielectric Strength | 19.6 kV/mm @Thickness 3.20 mm |
498 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics NORYL EN265 PPE+PS Extrusion grade. 254F (123C) DTUL. UL94 V-1 rated. |
|||
Dielectric Strength | 19.6 kV/mm | 499 kV/in | |
ACC QGel 300 QSI Quantum Silicones High Strength Gel QGel 300 is a clear, very soft, tough, moderately cross-linked, silicone polymer. Silicone gels are used to provide protection from vibration, thermal or mechanical shock. Silicone gels also provide.. |
|||
Dielectric Strength | 19.6 kV/mm @Thickness 3.17 mm |
498 kV/in @Thickness 0.125 in |
|
Advanced Elastomer Systems Santoprene® 251-85 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Dielectric Strength | 19.6 kV/mm @Thickness 3.17 mm |
498 kV/in @Thickness 0.125 in |
|
Advanced Elastomer Systems Santoprene® 251-92 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Dielectric Strength | 19.6 kV/mm @Thickness 3.20 mm |
498 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics NORYL ENG265 PPE+PS PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a.. |