Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.1 kV/mm | 434 kV/in | 60Hz, Short Time, dry; ASTM D149 |
Sumitomo Bakelite North America E 8353-706R-1 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Dielectric Strength | 17.1 kV/mm | 435 kV/in | |
Master Bond EP46HT Epoxy Adhesive for Structural Bonding Description: Master Bond System EP46HT is a newly formulated two component high performance heat resistant epoxy resin system with excellent mechanical strength and chemically resistant properties f.. |
|||
Dielectric Strength | 17.1 kV/mm | 435 kV/in | |
Master Bond EP46HT-1 Epoxy For Serviceability Up To 600°F Description: Master Bond EP46HT-1 is a two component epoxy system for high performance structural bonding and sealing suitable for applications where resistance to temperatures from -100°F to +550°.. |
|||
Dielectric Strength | 17.1 kV/mm @Thickness 3.17 mm |
435 kV/in @Thickness 0.125 in |
|
Master Bond EP46HT-2Med Two Component Heat Resistant Biocompatible Epoxy System Master Bond Polymer System EP46HT-2MED is a two component medical grade epoxy system for high performance structural bonding and casting suitable for applications where resistance to temperatures fr.. |
|||
Dielectric Strength | 17.1 kV/mm | 435 kV/in | |
Tra-Con Tra-Bond 2135D High Impact Epoxy Adhesive TRA-BOND 2135D is a medium viscosity epoxy adhesive recommended for bonding, laminating, sealing, and structural repair applications where easy mixing and good wetting combined with high impact stre.. |
|||
Dielectric Strength | 17.1 kV/mm | 434 kV/in | Short Time; ASTM D149 |
Plenco 6500 Phenolic, Briquette, Transfer Molded PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 .. |
|||
Dielectric Strength | 17.1 kV/mm | 435 kV/in | ASTM D149 |
3M Scotchcast™ 3570G-N Connector Sealing Pack The 3M Scotchcast Connector Sealing Pack 3570G-N insulates and provides protection for electrical spring connectors against dust, soil, water, and other environmental elements. Each sealing pack con.. |
|||
Dielectric Strength | 17.1 kV/mm | 434 kV/in | |
Dow Corning 3110 SILICONE RUBBER ENCAPSULANT Two-part, white, condensation cure, moderate flow, general purpose encapsulant, cure speed varied by catalyst type and mix ratio.Information provided by Dow Corning |
|||
Dielectric Strength | 17.1 kV/mm | 434 kV/in | Wet, short term. ASTM D149 |
Sumitomo Bakelite North America FS-80-P-1 Long-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GI.. |