Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 103 PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV stabilized for outdoor and lighting. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 103R PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 104 PC UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 104 PC (Asia Pacific) LEXAN 104 is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 121 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small intricate parts. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 123R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 124 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not .. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 131 PC (Asia Pacific) Nonhalogenated. 3.5 MFR. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 133 PC Nonhalogenated. 3.5 MFR. UV-stabilized. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 153R PC Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized. Internal mold release. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 153R PC (Asia Pacific) Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized. Internal mold release. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 201R PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. Internal mold release. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Lexan® 221 PC 17.5 MFR, for small, intricate parts. Improved flame retardance.This data was supplied by SABIC-IP for the Americas region. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 221R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 241R PC (Asia Pacific) 10.5 MFR. Improved flame retardance. Internal mold release. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 244RF PC (Asia Pacific) LEXAN 244RF resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP6NR PC (Europe-Africa-Middle East) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® LI1813R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release and UV-stabilized. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 141 PC (Asia Pacific) Nonhalogenated. 10.5 MFR. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Lexan® 141S PC (Asia Pacific) Nonhalogenated. 10.5 MFR. Internal mold release.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 143 PC (Asia Pacific) Nonhalogenated. 10.5 MFR. UV-stabilized. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 143R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. UV-stabilized. Internal mold release. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 144R PC (Asia Pacific) LEXAN 144R is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Lexan® 151 PC Nonhalogenated. 2.5 MFR. Blowmolding/extrusion.This data was supplied by SABIC-IP for the Americas region. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP6NR PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Dielectric Strength | 14.9 - 20.2 kV/mm | 378 - 513 kV/in | Average value: 17.9 kV/mm Grade Count:6 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP4NR PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |
|||
Dielectric Strength | 14.9 kV/mm @Thickness 3.20 mm |
378 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HP4NR PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |