Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.1 kV/mm @Thickness 1.00 mm |
358 kV/in @Thickness 0.0394 in |
in oil; ASTM D149 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 LNP* Konduit* PX08322 is a compound based on PA6 resin containing mineral. Added features include: Thermally Conductive, Flame Retardant |
|||
Dielectric Strength | 14.1 kV/mm @Thickness 1.00 mm |
358 kV/in @Thickness 0.0394 in |
in oil; ASTM D149 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Dielectric Strength | 14.1 kV/mm @Thickness 1.00 mm |
358 kV/in @Thickness 0.0394 in |
in oil; ASTM D149 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral filled PA6 non-halogen FR compound |
|||
Dielectric Strength | 14.1 kV/mm @Thickness 1.59 mm |
357 kV/in @Thickness 0.0625 in |
Unconditioned; ASTM D149 |
Garlock GYLON® 3594 PTFE Gasketing, Glass Fiber Filled PTFE with glass fiber fillerInformation provided by Garlock Rubber Technologies |
|||
Dielectric Strength | 14.1 kV/mm | 358 kV/in | Short Time; ASTM D149 |
Plenco 2311 Phenolic, Granular, Compression Molded PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr.. |
|||
Dielectric Strength | 14.1 kV/mm | 358 kV/in | Short Time; ASTM D149 |
Plenco 6990 Phenolic, Briquette, Injection Molded PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Dielectric Strength | 14.1 kV/mm | 358 kV/in | |
Covestro Desmopan® 150 Thermoplastic Polyurethane Desmopan 150 is a TPU on the basis of a standard ester.Applications: Ski boots, castors, shoe heels, technical injection molding parts.Information provided by Bayer.As of 1 September 2015, Bayer Mat.. |
|||
Dielectric Strength | 14.1 kV/mm | 358 kV/in | ASTM D149-97a |
DSM Somos® 9420 Epoxy Resin for Stereolithography DescriptionDSM Somos® 9420 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance and a wid.. |
|||
Dielectric Strength | 14.1 - 16.1 kV/mm | 359 - 409 kV/in | short time |
Bulk Molding Compounds BMC A20-(a) High Strength Grade Molding Compound BMC A20 is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A20 is well suited for injection, transfer or compression molding o.. |
|||
Dielectric Strength | 14.1 - 23.7 kV/mm | 358 - 602 kV/in | Average value: 18.6 kV/mm Grade Count:8 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |