Electrical Properties Metric English Comments
Dielectric Strength 1.00 - 14.6 kV/mm
25.4 - 371 kV/in
Average value: 5.72 kV/mm Grade Count:7
Overview of materials for Phenolic, Novolac, Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu..
Dielectric Strength 1.00 - 100 kV/mm
25.4 - 2540 kV/in
Average value: 33.0 kV/mm Grade Count:193
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Dielectric Strength 1.00 kV/mm

@Diameter >=3.00 mm
25.4 kV/in

@Diameter >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola Etronit B 65 Phenolic, Paper Reinforcement, Dark Brown, Tubes
Description: For mechanical and electrical low-voltage applications. Good electrical properties at normal air humidity.Applications: Winding tubes in the foil and metal foil industries and carrier t..
Dielectric Strength 1.00 kV/mm

@Diameter >=3.00 mm
25.4 kV/in

@Diameter >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola Etronit IV C Phenolic, Paper Reinforcement, Yellow, Tubes
Description: Suitable for electrical and mechanical applications where there is high air humidity. Lowest water absorption of all the Etronit types. Tropical grade. Good electrical properties at hig..
Dielectric Strength 1.00 kV/mm

@Diameter >=3.00 mm
25.4 kV/in

@Diameter >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola Etronit IV C S Phenolic, Paper Reinforcement, Black, Tubes
Description: Suitable for electrical and mechanical applications where there is high air humidity. Lowest water absorption of all the Etronit types. Tropical grade. Good electrical properties at hig..
Dielectric Strength 1.00 kV/mm
25.4 kV/in
Arkema Group Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Conditioned)
Designation ISO 1874-PA12,M,16-090,CF20Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on av..
Dielectric Strength 1.00 kV/mm
25.4 kV/in
Arkema Group Rilsan® ASR 30 Nylon 12, 30% Carbon Fiber Filled (Conditioned)
Designation ISO 1874-PA12,M,16-120,CF30Rigid grade with carbon fiber filler (30%) for injection molding. Available color: black.Very high rigidity. High strength-to-weight ratio. Very low shrinkage:..