Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | >= 0.00 sec @Thickness 3.05 mm |
>= 0.00 sec @Thickness 0.120 in |
UL PLC 0 |
Resinoid 7051 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Hot Wire Ignition, HWI | 0.00 - 7.0 sec @Thickness 1.50 mm |
0.00 - 7.0 sec @Thickness 0.0591 in |
UL 746A |
Idemitsu Kosan Xarec® N WA 7020 SPS, 20% Glass Filled Crystalline Polymer Blend, Glass Filled, Impact Modified. Used in Automotive Electronics applications. |
|||
Hot Wire Ignition, HWI | 0.00 - 2.0 sec | 0.00 - 2.0 sec | UL 746A |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Europe-Africa-Middle East) LNP VERTON* RV00AES is a compound based on PA 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Hot Wire Ignition, HWI | 0.00 - 2.0 sec | 0.00 - 2.0 sec | UL 746A |
SABIC Innovative Plastics LNP VERTON RV00AESS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized. |
|||
Hot Wire Ignition, HWI | 0.00 - 7.0 sec | 0.00 - 7.0 sec | UL 746A |
SABIC Innovative Plastics NORYL GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Hot Wire Ignition, HWI | 0.00 sec @Thickness >=0.750 mm |
0.00 sec @Thickness >=0.0295 in |
ASTM D3874-88 |
BASF Ultramid® A3XZG5 BK 23187 25% Glass Filled PA66 FR (Conditioned) Description: Impact-modified, 25% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; for compone.. |
|||
Hot Wire Ignition, HWI | >= 0.00 sec @Thickness 3.05 mm |
>= 0.00 sec @Thickness 0.120 in |
UL PLC 0 |
Resinoid 2016 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Hot Wire Ignition, HWI | >= 0.00 sec @Thickness 3.05 mm |
>= 0.00 sec @Thickness 0.120 in |
UL PLC 0 |
Resinoid 7201 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |