Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Curie Temperature 750 °C
1380 °F
Carpenter Chrome Core® 12 Alloy
Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen..
Curie Temperature 750 °C
1380 °F
Carpenter Chrome Core® 8 Alloy
Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen..
Curie Temperature 750 °C
1380 °F
Alliance S-20A Samarium Cobalt Magnetic Material
Curie Temperature 750 °C
1380 °F
Alliance S-20B Samarium Cobalt Magnetic Material
Curie Temperature 750 °C
1380 °F
Alliance S-26A Samarium Cobalt Magnetic Material
Curie Temperature 750 °C
1380 °F
Alliance S-26B Samarium Cobalt Magnetic Material
Curie Temperature 750 °C
1380 °F
Alliance S-28A Samarium Cobalt Magnetic Material
Curie Temperature 750 °C
1380 °F
Alliance S-28B Samarium Cobalt Magnetic Material
Curie Temperature 750 °C
1380 °F
Alliance S-30A Samarium Cobalt Magnetic Material
Curie Temperature 750 °C
1380 °F
Alliance S-30B Samarium Cobalt Magnetic Material
Curie Temperature 750 °C
1380 °F
Carpenter Chrome Core® 8-FM Alloy
Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen..
Curie Temperature 750 °C
1380 °F
Alliance S-28H Samarium Cobalt Magnetic Material
Curie Temperature 750 °C
1380 °F
Alliance S-32 Samarium Cobalt Magnetic Material
Curie Temperature 750 °C
1380 °F
Alliance S-22A Samarium Cobalt Magnetic Material
Curie Temperature 750 °C
1380 °F
Alliance S-26H Samarium Cobalt Magnetic Material
Curie Temperature 750 °C
1380 °F
Carpenter Chrome Core® 12-FM Alloy
Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen..
Curie Temperature 750 °C
1380 °F
Alliance S-22B Samarium Cobalt Magnetic Material