Electrical Properties Metric English Comments
Curie Temperature 450 °C
842 °F
Piezo Kinetics PKI 100 Lead Metaniobate Piezoelectric
Lead Metaniobate exhibits properties not usually present in other types of piezoelectric ceramics. The noteworthy facts are its low mechanical QM, negligible aging, wide range of operating temperat..
Curie Temperature 450 - 500 °C
842 - 932 °F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Curie Temperature 450 - 500 °C
842 - 932 °F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C)
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Curie Temperature 450 - 500 °C
842 - 932 °F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Cold-Rolled
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Curie Temperature 450 - 500 °C
842 - 932 °F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Curie Temperature 450 - 500 °C
842 - 932 °F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, After Process Annealed at 1600°F (871°C)
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Curie Temperature 450 - 500 °C
842 - 932 °F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Curie Temperature 450 - 500 °C
842 - 932 °F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C)
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Curie Temperature 450 - 500 °C
842 - 932 °F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Cold-Rolled
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Curie Temperature 450 - 500 °C
842 - 932 °F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Curie Temperature 450 °C
842 °F
Goodfellow Nickel/Iron/Molybdenum Alloy
Information provided by Goodfellow.
Curie Temperature 450 °C
842 °F
Alliance BIF-11 Bonded (Composite) Magnetic Material
Curie Temperature 450 °C
842 °F
Alliance BIF-17 Bonded (Composite) Magnetic Material
Curie Temperature 450 °C
842 °F
Alliance BIF-19 Bonded (Composite) Magnetic Material
Curie Temperature 450 °C
842 °F
Alliance BIF-2 Bonded (Composite) Magnetic Material
Curie Temperature 450 °C
842 °F
Alliance C-5 Strontium Ferrite Ceramic Magnetic Material
Curie Temperature 450 °C
842 °F
Alliance C-7 Strontium Ferrite Ceramic Magnetic Material
Curie Temperature 450 °C
842 °F
Alliance C-7B Strontium Ferrite Ceramic Magnetic Material
Curie Temperature 450 °C
842 °F
Alliance C-8 Strontium Ferrite Ceramic Magnetic Material
Curie Temperature 450 °C
842 °F
Alliance C-8H Strontium Ferrite Ceramic Magnetic Material
Curie Temperature 450 °C
842 °F
Alliance C-9 Strontium Ferrite Ceramic Magnetic Material
Curie Temperature 450 °C
842 °F
Alliance C-9B Strontium Ferrite Ceramic Magnetic Material
Curie Temperature 450 °C
842 °F
Alliance BIF-16 Bonded (Composite) Magnetic Material
Curie Temperature 450 °C
842 °F
Alliance C-8B Strontium Ferrite Ceramic Magnetic Material
Curie Temperature 450 °C
842 °F
PPT BP40 NiZn Ferrite Powder
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H..
Curie Temperature 450 - 500 °C
842 - 932 °F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, After Process Annealed at 1600°F (871°C)
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..