Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 1.20 kV/mm @Thickness >=3.00 mm |
30.5 kV/in @Thickness >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2 |
Elektro-Isola Etronit II Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: Mechanical and electrical applications used at normal air humidity. Very good electrical values.Information provided by Elektro-Isola |
|||
Dielectric Strength | 1.20 kV/mm @Thickness >=3.00 mm |
30.5 kV/in @Thickness >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2 |
Elektro-Isola Etronit IV C Phenolic, Paper Reinforcement, Yellow, Sheets Description: Grade for mechanical electrotechnical and high frequency purposes. Tropical grade, well suited for areas where high air humidity can be expected and lasting electrical properties despit.. |
|||
Dielectric Strength | 1.20 kV/mm @Thickness >=3.00 mm |
30.5 kV/in @Thickness >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr.. |