Electrical Properties Metric English Comments
Dielectric Strength 13.2 kV/mm

@Frequency 60.0 Hz
335 kV/in

@Frequency 60.0 Hz
step-by-step, wet; ASTM D149
Sumitomo Bakelite North America E 2748-9641D Short Glass Fiber Reinforced Epoxy
E 2748-9641D is a mineral and short fiberglass filled epoxy molding compound.Information provided by Sumitomo Bak North America, Inc.
Dielectric Strength 13.2 kV/mm

@Frequency 60.0 Hz
335 kV/in

@Frequency 60.0 Hz
step-by-step, wet; ASTM D149
Sumitomo Bakelite North America Epiall® 2061B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Epiall 2061B-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by S..