Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 90 dB | 90 dB | |
Premix Thermoplastics PRESEAL 5020 Ni-Coated Graphite Highly conductive PRESEAL® thermoplastic elastomer compounds are injection-mouldable and extrudable plastics for EMI-gasket and -housing applications, among other uses. The material is an ideal cho.. |
|||
Shielding Effectiveness | 90 dB | 90 dB | |
Premix Thermoplastics PRESEAL 5020 Ni-Coated Graphite Metal replacement is one of the fastest growing areas for conductive plastics. Plastics, with their lighter weight, good processability and optimal combination of mechanical properties have challeng.. |
|||
Shielding Effectiveness | 90 dB | 90 dB | ISO ARP1705, 20-700 MHz |
Premix Thermoplastics PRESEAL® TPE 5010 PRESEAL TPE 5010 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors or in grounding applica.. |
|||
Shielding Effectiveness | 90 dB | 90 dB | 20-700MHz; ARP1705 |
Premix Thermoplastics PRESEAL® TPE 5020 General Description:PRESEAL® TPE 5020 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors o.. |
|||
Shielding Effectiveness | 90 dB | 90 dB | ASTM D790 |
Premix Thermoplastics PRESEAL® TPE 5020 General Description:PRESEAL® TPE 5020 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors o.. |
|||
Shielding Effectiveness | >= 90 dB @Frequency 2.00e+9 Hz |
>= 90 dB @Frequency 2.00e+9 Hz |
Plane Wave; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1350 Conductive Elastomer Standard material for high volume injection and compression molding and small extrusions; high performance in non-corrosive environments; used in grounding applications with little or no vibration.R.. |
|||
Shielding Effectiveness | >= 90 dB | >= 90 dB | 2 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1485 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 90 dB | >= 90 dB | 2 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1501 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 90 dB | >= 90 dB | 500 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL E6306 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 90 dB | >= 90 dB | 20MHz - 10GHz; MIL-G-83528 |
Parker Chomerics CHO-SEAL® E6434E Conductive EPDM Elastomer Extruded Conductive EPDM Elastomer. This is an extruded conductive elastomer engineered for resistance to harsh chemicals, specifically those associated with decontaminates for military Nuclear, Bio.. |
|||
Shielding Effectiveness | <= 90 dB | <= 90 dB | |
Parker Chomerics SOFT-SHIELD® 7000 Low Closure Force EMI Gasket Designed where the gasket sees high level of compression cycles and/or greater than 70°CInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 90 dB | >= 90 dB | 10 GHz (Plane Wave) - Base/Reinforced Material; MIL-G-83528 |
Parker Chomerics CHO-SEAL 1287R Reinforced Conductive Elastomer Seal These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at.. |
|||
Shielding Effectiveness | <= 90 dB | <= 90 dB | Modified IEEE-299 |
Parker Chomerics CHOFORM® 5560 Conductive Form-in-Place Gasket Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Shielding Effectiveness | <= 90 dB | <= 90 dB | |
Parker Chomerics SOFT-SHIELD® 4005 Low Closure Force EMI Gasket Information provided by Chomerics |