Electrical Properties Metric English Comments
Static Decay 0.0100 - 2.00 sec
0.0100 - 2.00 sec
Average value: 1.03 sec Grade Count:7
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Static Decay 0.0100 - 2.00 sec
0.0100 - 2.00 sec
Average value: 0.543 sec Grade Count:5
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Static Decay 0.0100 - 2.00 sec
0.0100 - 2.00 sec
Average value: 0.396 sec Grade Count:5
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Static Decay 0.00300 - 2.00 sec
0.00300 - 2.00 sec
Average value: 1.38 sec Grade Count:6
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.32 sec Grade Count:5
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.77 sec Grade Count:26
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu..
Static Decay 0.0100 - 2.00 sec
0.0100 - 2.00 sec
Average value: 1.00 sec Grade Count:8
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max..
Static Decay 0.0100 - 2.00 sec
0.0100 - 2.00 sec
Average value: 0.862 sec Grade Count:17
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Static Decay 0.0500 - 2.00 sec
0.0500 - 2.00 sec
Average value: 1.33 sec Grade Count:8
Overview of materials for Polycarbonate, Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.84 sec Grade Count:19
Overview of materials for Polycarbonate, NCG Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr..
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.48 sec Grade Count:51
Overview of materials for Polycarbonate, Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val..
Static Decay 0.0100 - 2.00 sec
0.0100 - 2.00 sec
Average value: 0.921 sec Grade Count:12
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 0.875 sec Grade Count:4
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.81 sec Grade Count:8
Overview of materials for Polyphenylene Sulfide (PPS), Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum ..
Static Decay 1.00 - 2.00 sec
1.00 - 2.00 sec
Average value: 1.67 sec Grade Count:3
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.62 sec Grade Count:5
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.72 sec Grade Count:12
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
Static Decay 0.00200 - 2.00 sec
0.00200 - 2.00 sec
Average value: 1.50 sec Grade Count:4
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.68 sec Grade Count:6
Overview of materials for PC/ABS + Stainless Steel
This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.50 sec Grade Count:9
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.00 sec Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a..
Static Decay 1.00 - 2.00 sec
1.00 - 2.00 sec
Average value: 1.80 sec Grade Count:10
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.38 sec Grade Count:20
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo..
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.18 sec Grade Count:21
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.50 sec Grade Count:3
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Static Decay 0.0100 - 2.00 sec
0.0100 - 2.00 sec
Average value: 1.04 sec Grade Count:48
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..
Static Decay 1.00 - 2.00 sec
1.00 - 2.00 sec
Average value: 1.86 sec Grade Count:7
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.51 sec Grade Count:7
Overview of materials for Polypropylene, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o..
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.50 sec Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..
Static Decay 0.0100 - 2.00 sec
0.0100 - 2.00 sec
Average value: 1.00 sec Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu..
Copyright © lookpolymers.com All Rights Reserved