Polymer Property : Static Decay = 0.100 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.32 sec Grade Count:5
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.48 sec Grade Count:51
Overview of materials for Polycarbonate, Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val..
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.62 sec Grade Count:5
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.72 sec Grade Count:12
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.68 sec Grade Count:6
Overview of materials for PC/ABS + Stainless Steel
This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro..
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.38 sec Grade Count:20
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo..
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.18 sec Grade Count:21
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max..
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.51 sec Grade Count:7
Overview of materials for Polypropylene, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o..