Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | >= 200 sec | >= 200 sec | ASTM D495 |
Network Polymers Kepital® F10-02 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Arc Resistance | >= 200 sec | >= 200 sec | ASTM D495 |
Network Polymers Kepital® F20-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Arc Resistance | >= 200 sec | >= 200 sec | ASTM D495 |
Network Polymers Kepital® F20-52 Description: Natural Acetal Copolymer, Weather Resistance GradeInformation provided by Network Polymers Inc. |
|||
Arc Resistance | >= 200 sec | >= 200 sec | ASTM D495 |
Network Polymers Kepital® F30-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Arc Resistance | >= 200 sec | >= 200 sec | ASTM D495 |
Network Polymers Kepital® F40-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Arc Resistance | >= 200 sec | >= 200 sec | ASTM D495 |
Kolon Kocetal® DP301 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Arc Resistance | >= 200 sec | >= 200 sec | ASTM D495 |
Kolon Kocetal® VT701 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Arc Resistance | 200 sec @Thickness 3.17 mm |
200 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP159 Synthetic Fabric
(discontinued **) Description: Woven aramid fiber fabric combined with high temperature phenolic resin. With a proper post baking procedure, NP159 will withstand continuous operation at 200° C. Material becomes brit.. |
|||
Arc Resistance | >= 200 sec | >= 200 sec | ASTM D495 |
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Arc Resistance | >= 200 sec | >= 200 sec | ASTM D495 |
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Arc Resistance | 200 sec | 200 sec | ASTM D495 |
Sumitomo Bakelite North America SI 9002N-1 Silicone Compound Short fibergass reinforced silicone molding compound which offers moderate strength properties, dimensional stability, and excellent long-term thermal stability at elevated temperatures.Information .. |
|||
Arc Resistance | >= 200 sec | >= 200 sec | ASTM D495 |
Master Bond EP112M Two Component, Medium Viscosity Heat Curing Cycloaliphatic Epoxy Resin Product Description: Master Bond Polymer System EP112M is a solventless, medium viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor .. |
|||
Arc Resistance | 200 sec | 200 sec | |
Dow Corning 5-8601 FLUOROSILICONE LSR, KIT Fluorosilicone rubber designed for liquid injection moldingInformation provided by Dow Corning |
|||
Arc Resistance | 200 sec | 200 sec | ASTM D495 |
Sumitomo Bakelite North America SI 9002J-1 Silicone Compound SI 9002J-1 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated temp.. |