Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 170 sec | 170 sec | ASTM D495 |
Plenco 4100 Phenolic, Granular, Compression Molded
(discontinued **) Two-stage Phenolic. PLENCO 04100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in appliance and .. |
|||
Arc Resistance | 170 sec | 170 sec | ASTM D495 |
Sumitomo Bakelite North America 2004B Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Arc Resistance | 170 sec | 170 sec | |
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Injection Grade Sumikon PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Arc Resistance | 170 sec | 170 sec | ASTM D495 |
Plenco 4349 Phenolic, Granular, Transfer Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Arc Resistance | >= 170 sec | >= 170 sec | |
Bulk Molding Compounds BMC 606 Mineral Filled, Glass Reinforced Polyester Compound BMC 606 is a mineral filled, glass reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good moldability, excellent impact strength,.. |
|||
Arc Resistance | 170 sec | 170 sec | IPC TM-650 2.5.1 |
Arlon 33N Polyimide Laminate and Prepreg High reliability and high temperature material33N is a flame retardant polyimide laminate and prepreg system where the excellent high performance properties of polyimide need to be combined with fla.. |
|||
Arc Resistance | 170 sec | 170 sec | |
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Compression Grade Sumikon PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional sta.. |