Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Surface Resistivity per Square = 1.00e+7 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+7 - 1.00e+10 ohm
1.00e+7 - 1.00e+10 ohm
ASTM D257
Quadrant EPP TIVAR® CleanStat™ FDA, USDA, 3-A Dairy, Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet)
Surface Resistivity per Square <= 1.00e+7 ohm
<= 1.00e+7 ohm
ASTM D257
PolyOne Stat-Tech™ LC-40CF/000 Natural LCP (Liquid Crystal Polymer), 40% Carbon Fiber Reinforced, Electrically Conductive, EMI/RFI Shielding
Information provided by PolyOne™ Corporation
Surface Resistivity per Square >= 1.00e+7 ohm
>= 1.00e+7 ohm
VDE 0303
GEHR Plastics PEEK-mod Polyetheretherketone, 10% PTFE, 10% Graphite, 10% Carbon Fiber
Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical ..
Surface Resistivity per Square 1.00e+7 ohm
1.00e+7 ohm
after 200% elongation; ASTM D257
Kostat ICP-STAT ICS-1001 PET Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1.00e+7 ohm
1.00e+7 ohm
after 200% elongation; ASTM D257
Kostat ICP-STAT ICS-1003 PS Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1.00e+7 ohm
1.00e+7 ohm
after 200% elongation; ASTM D257
Kostat ICP-STAT ICS-1005 ABS Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1.00e+7 ohm
1.00e+7 ohm
after 200% elongation; ASTM D257
Kostat ICP-STAT ICD-1003 PS Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1.00e+7 ohm
1.00e+7 ohm
after 200% elongation; ASTM D257
Kostat ICP-STAT ICS-1000 PC Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Surface Resistivity per Square 1e+05 - 1.00e+7 ohm
1e+05 - 1.00e+7 ohm
ASTM D257
Diamond Polymers NPP25-0103 CF15 Conductive Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Surface Resistivity per Square 1e+05 - 1.00e+7 ohm
1e+05 - 1.00e+7 ohm
ASTM D257
Diamond Polymers NPP25-1111 CF15 Conductive Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Surface Resistivity per Square 1e+05 - 1.00e+7 ohm
1e+05 - 1.00e+7 ohm
ASTM D257
CEN® Electronic Material BX Polyimide Film
CEN®BX Polyimide Film are electrically conductive, and are precisely loaded with conductive fillers to produce films with tightly controlled surface resistivities. BX films provide both thermal and..
Surface Resistivity per Square 1.00e+7 - 1.20e+8 ohm
1.00e+7 - 1.20e+8 ohm
Atom Adhesives AA-DUCT 905 Epoxy Adhesive
AA-DUCT 905 is a single component epoxy, formulated with pure silver powder combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive..