Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+10 ohm | >= 1.00e+10 ohm | ASTM D257 |
Quadrant EPP TIVAR® Polysteel Filled UHMW-PE, High Specific Gravity (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | 1.00e+10 ohm | 1.00e+10 ohm | ASTM D257 |
Kostat G148BK TAB Spacer Reels KOSTATs TAB Spacer Reels are ideal for shipment and storage of any components packaged in TAB spacer tapes. KOSTATSs TAB Spacer Reels, uniquely formulated and manufactured with the most advanced in.. |
|||
Surface Resistivity per Square | 1.00e+10 ohm | 1.00e+10 ohm | 12% Humidity; ASTM D257 |
Ex-Tech Plastics PerformaTech™ PVC XSD-28 Static Dissipative PVC Manufactured in thickness from 10 to 60 mils, PerformTech XSD-28 is available in rigid vinyl or PET. XSD-28 is a static dissipative sheet engineered specifically for ESD sensitive packaging for use .. |
|||
Surface Resistivity per Square | 1.00e+10 ohm @Temperature 20.0 °C |
1.00e+10 ohm @Temperature 68.0 °F |
500 V DC @ 60% RH; ASTM D257 |
DuPont Teijin Films Melinex® 539 Polyester Film, 370 Gauge Melinex® 539 is a two sided treated grade of clear film for applications where freedom from static is required. Its main use is as a montage "foil" in the production of printing plates. Melinex® 5.. |
|||
Surface Resistivity per Square | 1.00e+10 ohm @Temperature 20.0 °C |
1.00e+10 ohm @Temperature 68.0 °F |
500 V DC @ 60% RH; ASTM D257 |
DuPont Teijin Films Melinex® 539 Polyester Film, 700 Gauge Melinex® 539 is a two sided treated grade of clear film for applications where freedom from static is required. Its main use is as a montage "foil" in the production of printing plates. Melinex® 5.. |