Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 180 - 225 V | 180 - 225 V | Average value: 191 V Grade Count:10 |
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum .. |
|||
Comparative Tracking Index | 150 - 225 V | 150 - 225 V | Average value: 177 V Grade Count:32 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
Comparative Tracking Index | 200 - 225 V | 200 - 225 V | Average value: 217 V Grade Count:6 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is.. |