Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 20.0 °C |
0.0001033 ohm-cm @Temperature 68.0 °F |
|
Latrobe MP35N® Alloy MP35N is a nickel-cobalt base alloy of the Multiphase alloy system that has a unique combination of properties - ultra high strength, toughness, ductility, and outstanding corrosion resistance. The .. |
|||
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 23.0 °C |
0.0001033 ohm-cm @Temperature 73.4 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 23.0 °C |
0.0001033 ohm-cm @Temperature 73.4 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 23.0 °C |
0.0001033 ohm-cm @Temperature 73.4 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 15% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 23.0 °C |
0.0001033 ohm-cm @Temperature 73.4 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 15% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 23.0 °C |
0.0001033 ohm-cm @Temperature 73.4 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 25% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 23.0 °C |
0.0001033 ohm-cm @Temperature 73.4 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 25% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 23.0 °C |
0.0001033 ohm-cm @Temperature 73.4 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 35% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 23.0 °C |
0.0001033 ohm-cm @Temperature 73.4 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 35% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 23.0 °C |
0.0001033 ohm-cm @Temperature 73.4 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 45% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 23.0 °C |
0.0001033 ohm-cm @Temperature 73.4 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 45% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 23.0 °C |
0.0001033 ohm-cm @Temperature 73.4 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 53% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 23.0 °C |
0.0001033 ohm-cm @Temperature 73.4 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 55% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 23.0 °C |
0.0001033 ohm-cm @Temperature 73.4 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 65% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 23.0 °C |
0.0001033 ohm-cm @Temperature 73.4 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 33%, Aged 565°C/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Electrical Resistivity | 0.0001033 ohm-cm @Temperature 23.0 °C |
0.0001033 ohm-cm @Temperature 73.4 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 53%, Aged 565°C/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |