Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.00e+12 ohm | 2.00e+12 ohm | ASTM D257 |
Rogers Corporation Poron® 4701-40-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Surface Resistance | 2.00e+12 ohm | 2.00e+12 ohm | ASTM D257 |
Rogers Corporation Poron® 4701-40-30 Cellular Urethane Foam Information on this material is preliminary.Standard color is black (04); others are available. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F).General Poron® information: Poron® fo.. |
|||
Surface Resistance | 2.00e+12 ohm | 2.00e+12 ohm | IEC 60093 |
LG Chemical LUCON TR1000 PMMA+CNT Description: Injection Molding, PMMA+CNT, Transparency, Permanent Antistatic, Low OutgassingApplication: Wafer Carrier Cover, Pellicle TrayCAS No. 9010-94-0 and 25053-09-2Information provided by LG .. |
|||
Surface Resistance | 2.00e+12 ohm | 2.00e+12 ohm | |
Covestro Desmopan® 150 Thermoplastic Polyurethane Desmopan 150 is a TPU on the basis of a standard ester.Applications: Ski boots, castors, shoe heels, technical injection molding parts.Information provided by Bayer.As of 1 September 2015, Bayer Mat.. |
|||
Surface Resistance | 2.00e+12 ohm @Temperature 20.0 °C |
2.00e+12 ohm @Temperature 68.0 °F |
65% RH; ASTM D257 |
Arkema Group Pebax® 3533 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Surface Resistance | 2.00e+12 ohm | 2.00e+12 ohm | |
Arkema Group Rilsan® BECN P20 TL Nylon 11 (Conditioned) ISO data provided by the manufacturer, Arkema. |
|||
Surface Resistance | 2.00e+12 ohm | 2.00e+12 ohm | |
Arkema Group Rilsan® BESN P20 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EHL,22-004Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.Flexibility. High impact strength. Very good chemical resistan.. |
|||
Surface Resistance | 2.00e+12 ohm | 2.00e+12 ohm | |
Arkema Group Rilsan® BMN P20 D Nylon 11 (Conditioned) Designation ISO 1874-PA11-P,MR,12-004Flexible grade for injection molding. Available colors: black and natural. Mold release agent.Outstanding working properties. Easy filling of the mold due to its.. |
|||
Surface Resistance | 2.00e+12 ohm | 2.00e+12 ohm | |
XXXPC Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Surface Resistance | 2.00e+12 ohm | 2.00e+12 ohm | ASTM D257 |
Rogers Corporation Poron® 4701-40-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |