Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 1.25e+18 ohm
1.25e+18 ohm
ASTM D257
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
Surface Resistance 1.25e+18 ohm
1.25e+18 ohm
ROA; IEC 60093
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
Surface Resistance 1.25e+18 ohm
1.25e+18 ohm
ASTM D257
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
Surface Resistance 1.25e+18 ohm
1.25e+18 ohm
ROA; IEC 60093
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
Surface Resistance 1.25e+18 ohm
1.25e+18 ohm
ASTM D257
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...
Surface Resistance 1.25e+18 ohm
1.25e+18 ohm
ROA; IEC 60093
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity...