Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.16e+9 - 3.16e+10 ohm | 3.16e+9 - 3.16e+10 ohm | IS 3396-1979 |
Amity Thermosets ATG 115 Phenolic Molding Organic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic .. |
|||
Surface Resistance | 1.00e+10 - 3.16e+10 ohm | 1.00e+10 - 3.16e+10 ohm | IS 3396-1979 |
Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |
|||
Surface Resistance | 1.00e+10 - 3.16e+10 ohm | 1.00e+10 - 3.16e+10 ohm | IS 3396-1979 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni.. |
|||
Surface Resistance | 1.00e+10 - 3.16e+10 ohm | 1.00e+10 - 3.16e+10 ohm | IS 3396-1979 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication .. |