Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.30e+14 ohm-cm | 2.30e+14 ohm-cm | ASTM D257 |
Covestro Baydur® GS-772 Polyurethane Solid RIM, MDI-based 2-Component Liquid System 0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Electrical Resistivity | 2.30e+14 ohm-cm | 2.30e+14 ohm-cm | ASTM D257 |
CRP Technology Windform® FX Polyamide Composite Processed by selective laser sintering (SLS). Windform® FX is a new generation polyamide based material, whose repeatability and mechanical characteristics make it particularly suited for Additive.. |