Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.00e+13 - 1.50e+16 ohm-cm | 2.00e+13 - 1.50e+16 ohm-cm | Average value: 3.68e+15 ohm-cm Grade Count:18 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Electrical Resistivity | 1.00e+12 - 1.50e+16 ohm-cm | 1.00e+12 - 1.50e+16 ohm-cm | Average value: 6.25e+15 ohm-cm Grade Count:4 |
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Electrical Resistivity | 1.00e+7 - 1.50e+16 ohm-cm @Temperature 75.0 - 300 °C |
1.00e+7 - 1.50e+16 ohm-cm @Temperature 167 - 572 °F |
Average value: 3.36e+15 ohm-cm Grade Count:2 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |