Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 7.00e+13 - 1.00e+15 ohm-cm | 7.00e+13 - 1.00e+15 ohm-cm | Average value: 4.88e+14 ohm-cm Grade Count:6 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 7.00e+13 ohm-cm | 7.00e+13 ohm-cm | |
Covestro Baydur® GS PIR A Polyurethane PIR casting system for the production of solid components. Mechanical properties can be varied by adjusting the mixing ratio in the range 1:1-1:2.Information provided by Bayer.As of 1 September 2015.. |
|||
Electrical Resistivity | 7.00e+13 ohm-cm | 7.00e+13 ohm-cm | |
Covestro Baydur® GS PIR B Polyurethane PIR casting system for the production of solid components. Mechanical properties can be varied by adjusting the mixing ratio in the range 1:1-1:2.Information provided by Bayer.As of 1 September 2015.. |
|||
Electrical Resistivity | 7.00e+13 ohm-cm | 7.00e+13 ohm-cm | |
Arkema Group Rilsan® BZM 30 TL Nylon 11, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MHL,18-050,GF30Rigid grade with glass fiber (30%) filler for injection molding. Available colors: black and natural. Light and heat stabilized.Rigidity. High compressive st.. |