Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | |
Momentive Performance Materials RTV511 White Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Electrical Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | |
Momentive Performance Materials RTV560 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Electrical Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | |
Momentive Performance Materials RTV566 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Electrical Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | |
Arkema Group Orgalloy® LT 4060IH Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (200 MPa), good .. |
|||
Electrical Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | |
Arkema Group Kynar® FLEX 2750 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EG1NS, M. ?E7.B.F.A.C,, ? (4-10)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousne.. |
|||
Electrical Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | |
Arkema Group Kynar® FLEX 2800 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EG1N, N. ?E7.D.G.B.C,, ? (3.5-7.5)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, impervious.. |