Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco 10 AS WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco 10 WOLLASTOCOAT® Wollastonite Chemically treated grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco ASPECT® 3000 Wollastonite High aspect ratio grade. It is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. .. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco HARRP™ 20 X 40 Wollastonite HARRP™ 20X40 is suggested for concrete and concrete roof tile reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco HARRP™ 40 Wollastonite HARRP™ 40 is suggested for concrete, roof tile, grout/stucco, etc. reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distin.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco HARRP™ Coarse Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco M1250 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco M200 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco M3 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco M400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco MD400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYAD G® WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYAD® 1250 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYAD® 325 Wollastonite Powdered grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particl.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYAD® 5000 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYAD® 5000 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYAD® M100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYAD® M200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYAD® MD200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYAD® MG Wollastonite High aspect ratio grade. This grade is recommended for elastomer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinct.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYCOR® 100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYGLOS® 12 Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYGLOS® 20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYGLOS® 4W Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYGLOS® M15 Wollastonite High aspect ratio grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal perf.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYGLOS® M3 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco NYGLOS® STPO Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco RRIMGLOS® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco RRIMGLOS® II Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite |
Nyco ULTRAFIBRE® 30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |