Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+12 - 1.00e+16 ohm-cm | 1.00e+12 - 1.00e+16 ohm-cm | Average value: 2.33e+15 ohm-cm Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+16 ohm-cm | 1.00e+12 - 1.00e+16 ohm-cm | Average value: 2.63e+15 ohm-cm Grade Count:14 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Plenco 501 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 501 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in heat resistant and electrical applications. It is designed for elevated temperature exposure for e.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Plenco 504 Black (COM) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)< Plaslok 504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding compounds. Since it also has good electrical.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Plenco 504 Black (INJ) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)< Plaslok 504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding compounds. Since it also has good electrical.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Plaslok 202 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 202 is a two-stage, woodflour-filled .. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+15 ohm-cm | 1.00e+12 - 1.00e+15 ohm-cm | Average value: 3.00e+14 ohm-cm Grade Count:4 |
Overview of materials for Nylon 11, Cable Sheathing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | |
GBC Grade 92 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Sumitomo Bakelite Durez® 22257 Phenolic, Compression Grade Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. .. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Sumitomo Bakelite Durez® 29502 B Phenolic, Compression Grade Durez 29502 B brown phenolic is a two stage, glass and mineral filled, special purpose molding material with improved mechanical and heat resistant properties. It is formulated for close tolerance .. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Sumitomo Bakelite Durez® 31735 Phenolic, Compression Grade Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Sumitomo Bakelite Durez® 31906 Phenolic, Injection Grade Durez 31906 Black Phenolic is an asbestos free, medium impact, molding compound. It is designed for applications where additional mechanical strength is required.Information provided by Sumitomo Ba.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Sumitomo Bakelite Sumikon® PM-9640 Glass Filled Phenolic Two stage glass fiber filled black phenolic. It is especially designed for applications requiring high strength and dimensional stability with excellent heat resistance. PM-9640 is widely used in .. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | |
Arkema Group Rilsan® AESN P20 TL Nylon 12, Flexible Grade (Conditioned) Designation ISO 1874-PA12-P,EHL,22-005Flexible grade for overmolding. Available colors: natural and white. Light and heat stabilized. No lubricant.Flexibility. Very good ability to overmold Pebax an.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Chang Chun Plastic Longlite PM T359J General Purpose Phenolic Molding Compound ASTM Grades per ASTM D700 are 3, 14.Information provided by Dowell Trading Company Ltd. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | |
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | |
Arkema Group Rilsan® AZM 50 NOIR T6LD Nylon 12, 50% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-090,GF50Rigid grade with glass fiber (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Toyobo Pelprene™ P-30B Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+16 ohm-cm | 1.00e+12 - 1.00e+16 ohm-cm | Average value: 2.68e+15 ohm-cm Grade Count:12 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Plaslok 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 5000 is the replacement material for .. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Plaslok 504 Black (INJ) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)&l Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 504 is a two-stage, mineral and cellu.. |