Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0100 - 10000 ohm-cm | 0.0100 - 10000 ohm-cm | |
NanoAmor 50% Regular Single Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, and gas-discharge tubes in telecom networksElectromagnetic-wave absorption an.. |
|||
Electrical Resistivity | 0.0100 - 10000 ohm-cm | 0.0100 - 10000 ohm-cm | |
NanoAmor 95%, OD/ID: 20-40/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Electrical Resistivity | 0.0100 - 1.00e+16 ohm-cm | 0.0100 - 1.00e+16 ohm-cm | Average value: 2.76e+15 ohm-cm Grade Count:79 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Electrical Resistivity | 0.0100 - 1.00e+12 ohm-cm | 0.0100 - 1.00e+12 ohm-cm | Average value: 1.03e+10 ohm-cm Grade Count:59 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Electrical Resistivity | 0.0100 - 100 ohm-cm | 0.0100 - 100 ohm-cm | Average value: 22.6 ohm-cm Grade Count:9 |
Overview of materials for Polypropylene, Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu.. |
|||
Electrical Resistivity | <= 0.0100 ohm-cm @Temperature 65.6 - 150 °C |
<= 0.0100 ohm-cm @Temperature 150 - 302 °F |
Average value: 0.00364 ohm-cm Grade Count:5 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | <= 0.0100 ohm-cm @Time 900 - 10800 sec |
<= 0.0100 ohm-cm @Time 0.250 - 3.00 hour |
Average value: 0.00364 ohm-cm Grade Count:5 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 0.0100 - 200000 ohm-cm | 0.0100 - 200000 ohm-cm | Average value: 13200 ohm-cm Grade Count:17 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Electrical Resistivity | 0.0100 - 0.100 ohm-cm | 0.0100 - 0.100 ohm-cm | Applied Coating; formulated with DMSO or MEG |
Heraeus Cleviosâ„¢ P Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P is an antistatic material based on PEDOT:PSS.. |
|||
Electrical Resistivity | 0.0100 - 0.100 ohm-cm | 0.0100 - 0.100 ohm-cm | Applied Coating; formulated with DMSO or MEG |
Heraeus Cleviosâ„¢ PH Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ PH is an antistatic material based on PEDOT:PS.. |
|||
Electrical Resistivity | 0.0100 ohm-cm | 0.0100 ohm-cm | cured 24 hr at 25°C (77°F). Value is 0.003 Ohm-cm cured 3 hr at 65°C (150°F) |
Von Roll Isola IMI E-Solder® 3022 Electrically Conductive Adhesive Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t.. |
|||
Electrical Resistivity | 0.0100 ohm-cm | 0.0100 ohm-cm | |
Von Roll Isola IMI E-Solder® 3026 Electrically Conductive Adhesive Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t.. |
|||
Electrical Resistivity | 0.0100 - 1.00e+7 ohm-cm | 0.0100 - 1.00e+7 ohm-cm | Tailorable; ASTM D4496 |
Touchstone CFOAM® 25 Structural Carbon Foam CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins.. |
|||
Electrical Resistivity | 0.0100 - 5.00e+14 ohm-cm | 0.0100 - 5.00e+14 ohm-cm | Average value: 2.00e+14 ohm-cm Grade Count:4 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |