Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00100 - 8.10e+15 ohm-cm | 0.00100 - 8.10e+15 ohm-cm | Average value: 2.07e+15 ohm-cm Grade Count:32 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Electrical Resistivity | 0.00100 ohm-cm | 0.00100 ohm-cm | In-Plane |
GrafTech eGRAF® HITHERM™ HT-2505 Graphite with Polymer Additive Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Electrical Resistivity | 0.00100 ohm-cm | 0.00100 ohm-cm | In-Plane |
GrafTech eGRAF® HITHERM™ HT-2510 Graphite with Polymer Additive Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Electrical Resistivity | 0.00100 ohm-cm | 0.00100 ohm-cm | In-Plane |
GrafTech eGRAF® HITHERM™ HT-705 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Electrical Resistivity | 0.00100 ohm-cm | 0.00100 ohm-cm | In-Plane |
GrafTech eGRAF® HITHERM™ HT-710 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Electrical Resistivity | 0.00100 ohm-cm | 0.00100 ohm-cm | In-Plane |
GrafTech eGRAF® HITHERM™ HT-720 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Electrical Resistivity | 0.00100 ohm-cm | 0.00100 ohm-cm | In-Plane |
GrafTech eGRAF® HITHERM™ HT-1205 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Electrical Resistivity | 0.00100 ohm-cm | 0.00100 ohm-cm | In-Plane |
GrafTech eGRAF® HITHERM™ HT-1210 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Electrical Resistivity | 0.00100 ohm-cm | 0.00100 ohm-cm | In-Plane |
GrafTech eGRAF® HITHERM™ HT-1220 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Electrical Resistivity | 0.00100 ohm-cm | 0.00100 ohm-cm | |
Toho Tenax Besfight® G55-700 24K HMA-5C A303 Continuous Filament Carbon Fiber High Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon .. |
|||
Electrical Resistivity | 0.00100 ohm-cm | 0.00100 ohm-cm | |
Toho Tenax Besfight® G80-600 12K UMA-5C F301 Continuous Filament Carbon Fiber High Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon .. |
|||
Electrical Resistivity | 0.00100 ohm-cm | 0.00100 ohm-cm | |
Toho Tenax Besfight® G50-300 12K HMA-7C EP01 Continuous Filament Carbon Fiber High Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon .. |
|||
Electrical Resistivity | 0.00100 ohm-cm | 0.00100 ohm-cm | |
Toho Tenax Besfight® G60-600 12K UMA-5C A303 Continuous Filament Carbon Fiber High Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon .. |
|||
Electrical Resistivity | <= 0.00100 ohm-cm | <= 0.00100 ohm-cm | |
Epoxyset Epoxiohm EO-30M-1 Electrically Conductive Epoxy Adhesive EO-30M-1 is a two part, semi-rigid, silver filled, epoxy adhesive. EO-30M-1 exhibits superior adhesion to a wide variety of substrates including most metals, ceramics, glass and plastics.Information.. |
|||
Electrical Resistivity | 0.00100 - 0.00300 ohm-cm | 0.00100 - 0.00300 ohm-cm | |
Alliance BCN-11 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00100 - 0.00300 ohm-cm | 0.00100 - 0.00300 ohm-cm | |
Alliance BCN-13 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00100 - 1.00e+8 ohm-cm | 0.00100 - 1.00e+8 ohm-cm | |
BACT Metal-Dylyn® Diamond-Like Nanocomposite Coating Metal-doped Me/a-C:H/a-Si:O nanocomposite. The electrical characteristics of these coatings can be tailored by the addition of metal dopants. This creates an engineered surface for specialized ap.. |
|||
Electrical Resistivity | 0.00100 - 0.00300 ohm-cm | 0.00100 - 0.00300 ohm-cm | |
Alliance BCN-10 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00100 - 0.00300 ohm-cm | 0.00100 - 0.00300 ohm-cm | |
Alliance BCN-12 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00100 - 0.00300 ohm-cm | 0.00100 - 0.00300 ohm-cm | |
Alliance BCN-14 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00100 - 0.00300 ohm-cm | 0.00100 - 0.00300 ohm-cm | |
Alliance BCN-15 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | 0.00100 - 0.00300 ohm-cm | 0.00100 - 0.00300 ohm-cm | |
Alliance BCN-17 Bonded (Composite) Magnetic Material |