Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 321 - 329 °C | 610 - 624 °F | |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Melt Temperature | 316 - 329 °C | 601 - 624 °F | |
LNP Lubricomp® UFL-4036 HS Polyphthalamide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr.. |
|||
Melt Temperature | 316 - 329 °C | 601 - 624 °F | |
LNP Thermocomp® UC-1006 Polyphthalamide, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Melt Temperature | 316 - 329 °C | 601 - 624 °F | |
LNP Thermocomp® UF-1006 HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |
|||
Melt Temperature | 316 - 329 °C | 601 - 624 °F | |
LNP Thermocomp® UF-1009 HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Melt Temperature | 321 - 329 °C | 610 - 624 °F | |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Melt Temperature | 321 - 329 °C | 610 - 624 °F | |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Melt Temperature | 316 - 329 °C | 601 - 624 °F | |
LNP Lubricomp® BGU- Polyphthalamide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr.. |
|||
Melt Temperature | 316 - 329 °C | 601 - 624 °F | |
LNP Thermocomp® UF-1006 A HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |
|||
Melt Temperature | 316 - 329 °C | 601 - 624 °F | |
LNP Thermocomp® UF-1008 Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Melt Temperature | 316 - 329 °C | 601 - 624 °F | |
LNP Thermocomp® UFM-3249 HS BK8-115 Polyphthalamide, Glass Mineral Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |
|||
Melt Temperature | 316 - 329 °C | 601 - 624 °F | |
LNP Verton™ UF-700-10 Polyphthalamide, Long Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |