Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 149 - 279 °C | 300 - 534 °F | Average value: 219 °C Grade Count:177 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Melt Temperature | 170 - 279 °C | 338 - 534 °F | Average value: 222 °C Grade Count:70 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Melt Temperature | 170 - 279 °C | 338 - 534 °F | Average value: 217 °C Grade Count:15 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Melt Temperature | 241 - 279 °C | 466 - 534 °F | Injection |
Albis Plastics ASA 02A 811 Unreinforced
(discontinued **) Acrylonitrile/Styrene/AcrylateCharacteristics: Excellent UV, Good Rigidity, Good Dimensional StabilityApplications: Sunglasses, Boat Shells, Roofs for Campers & RVsProcessing: Injection Molding (Mel.. |
|||
Melt Temperature | 241 - 279 °C | 466 - 534 °F | Injection Molding |
Styrolution Luran® S 778 T ASA Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Melt Temperature | 241 - 279 °C | 466 - 534 °F | Injection |
Albis Plastics ASA 02A MR20 , 20% Mineral Filled
(discontinued **) Acrylonitrile/Styrene/AcrylateCharacteristics: Excellent UV, Good Rigidity, Good Dimensional StabilityApplications: Sunglasses, Boat Shells, Roofs for Campers & RVsProcessing: Injection Molding (Mel.. |
|||
Melt Temperature | 170 - 279 °C | 338 - 534 °F | Average value: 215 °C Grade Count:51 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Melt Temperature | 170 - 279 °C | 338 - 534 °F | Average value: 224 °C Grade Count:92 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Melt Temperature | 170 - 279 °C | 338 - 534 °F | Average value: 205 °C Grade Count:6 |
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |