Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 227 - 243 °C | 440 - 470 °F | Molding |
PolyOne Lubri-Tech™ AS-10GB/02S Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
(discontinued **)< Description/Features:Glass Bead FilledSilicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 221 - 243 °C | 430 - 470 °F | Molding |
PolyOne Edgetek® AS-30GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 221 - 243 °C | 430 - 470 °F | |
LTL Color Compounds ColorFast® ACR100IM Polymethylmethacrylate, High Impact High impact version, extrusion or injection molding PMMAAll information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 221 - 243 °C | 430 - 470 °F | |
MRC Polymers MAXTELâ„¢ 600T10-BK TPO, 10% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Melt Temperature | 221 - 243 °C | 430 - 470 °F | |
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol.. |
|||
Melt Temperature | 221 - 243 °C | 430 - 470 °F | |
MRC Polymers MAXTELâ„¢ 600-BK TPO, Black For automotive exterior applications. Excellent process ability and dimensional stability.Unfilled TPOAvailable in black and gray onlyCan be UV StabilizedInternal and external lubricants can be add.. |
|||
Melt Temperature | 232 - 243 °C | 450 - 470 °F | |
Techmer ES Electrafil® PS-31/EC BK Polystyrene, Electrically Conductive Carbon Black |
|||
Melt Temperature | 221 - 243 °C | 430 - 470 °F | Molding |
PolyOne Stat-Tech™ AS-30GF/000 SD Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedAntistaticInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 227 - 243 °C | 440 - 470 °F | Molding |
PolyOne Edgetek® AS-10GB/000 Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |