Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 238 - 254 °C | 460 - 490 °F | |
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | Molding |
PolyOne Edgetek® PS-15GF-25MN/000 Polybutylene Terephthalate (PBT), Glass/Mineral Filled
(discontinued **)< Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 238 - 277 °C | 460 - 531 °F | |
PolyOne Stat-Tech™ NY-20CF/000 BLACK Polyamide 6 (Nylon 6) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Melt Temperature | 238 - 288 °C | 460 - 550 °F | |
DuPont Bexloy® AXW602NC010 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin
(discontinued **) A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont. |
|||
Melt Temperature | 238 - 271 °C | 460 - 520 °F | Stock |
PolyOne Lubri-Tech™ NL-10GF/15TF Nylon 6/12 - 10% Glass Fiber - 15% PTFE Flock
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
MTI ThermoStran® TPU-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
Clariant Renol PA213 Nylon 6, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 238 - 260 °C | 460 - 500 °F | |
Clariant Renol PA233G13HT Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Melt Temperature | 238 - 280 °C | 460 - 536 °F | Average value: 258 °C Grade Count:30 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |
|||
Melt Temperature | 238 - 282 °C | 460 - 540 °F | Average value: 256 °C Grade Count:15 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |