Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 190 °C | 374 °F | |
Multibase TPSiV® 4000-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | |
Polykemi AB POLYasa 2410F High Flow ASA Information provided by Polykemi AB |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 2590 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Good balance of flow, strength and heat resistance, USP Class VIApplications: Consumer electronics, Housewares, Co-extrusion cap coat, Impact resin cuttingExposure to gamma radi.. |
|||
Melt Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical LUCEL VC127-LD Antistatic POM, Unreinforced, High Flow, For VCR Reels LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 1300 High Heat Crystal Polystyrene High heat resistance, High strength, Good processing characteristics, USP Class ViApplications: Electronics packaging, Medical packaging, Cosmetic cases, Profile extrusionExposure to gamma radiation.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 3100 General Purpose Crystal Polystyrene Good balance of flow and set-up properties, Good crack resistanceApplications: Single service cutlery, Single service drinkware, Consumer electronic packagingExposure to gamma radiation in the 2.02-.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 5410 High Impact Polystyrene High impact, Good ESCR, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverages cups, Custom sheetProperties were determined on injection molded specimens at 23°C .. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | |
LATI Lastilac AR G/17-V0E ABS, 17% Glass Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability.Availability: Afri.. |
|||
Melt Temperature | 190 - 210 °C | 374 - 410 °F | Extrusion |
Stellarchem LP-830 TPE Compound This grade of Stellarchem LP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Processing Temperature |
Teknor Apex Uniprene® 7010-64NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Processing Temperature |
Teknor Apex Uniprene® UN-1140A Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | Processing Temperature |
Teknor Apex Uniprene® UN-2420D Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Temperature | 190 - 250 °C | 374 - 482 °F | |
Borealis BorPURE™ MB6561 High Density Polyethylene for Injection Molding BorPure™ MB6561 is a bimodal, high-density polyethylene intended for injection and compression molding. This grade combines excellent organoleptic properties, environmental stress crack resistance .. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | pre-drying required |
Corbion Purac Blend B High Heat, High Modulus Homopolymer PLA Heat resistance higher than typical PLA is achieved by addition of a nucleating agent and PDLA homopolymer. Increased modulus is produced by addition of talc to the base grade. Data is for samples.. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | Extrusion |
Total XSene® XRC 20 B High Density Polyethylene - Pipes and Fittings This product is a Total Ecosolutions grade.HDPE XRC 20 B is a very high performance hexene-based black compound, with a MRS 10 MPa - PE100 classification, particularly appropriate for pressure pipes.. |
|||
Melt Temperature | 190 - 220 °C | 374 - 428 °F | Extrusion |
Polimeri Europa Edistir N 2982 Polystyrene General purpose polystyrene with very high flow and high heat resistance. Special grade for direct gassing extrusion of heavy gage insulating boards (XPS) foamed by blowing agents alternative to CFC.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 3510 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 3511 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure.. |
|||
Melt Temperature | 190 - 230 °C | 374 - 446 °F | |
BASF Ultraform S 1320 0021 UNC POM Ultraform S1320 0021 UNC is an easy flowing, rapidly freezing injection molding POM grade with enhanced stiffness and heat distortion resistance. It is highly stabilized to resist aggressive fuels,.. |
|||
Melt Temperature | 190 - 274 °C | 374 - 525 °F | |
Ineos Nova 1301 High Heat Crystal Polystyrene High heat resistance, High strength, Good processing characteristics, USP Class VIApplications: Electronics packaging, Medical packaging, Cosmetic cases, Profile extrusionExposure to gamma radiation.. |