Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable 0800-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible) NOTE: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable 1104L-xx61FRD Polyvinyl Chloride, Flexible (PVC, Flexible) NOTE: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information p.. |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable JJF102L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 182 °C | 331 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable JKC30A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable JLK51A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable JLK51L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable MJF114A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1104L-xx40D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1250L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable W2302 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJB593KBL Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJJX207L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJLK61 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 174 °C | 331 - 345 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJMF113L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Wire & Cable Y283 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 176 °C | 331 - 349 °F | |
PolyOne Geon™ Vinyl Wire & Cable Y594B Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Flexible B8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Flexible R295AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 166 - 177 °C | 331 - 351 °F | |
PolyOne Geon™ Vinyl Flexible R7542X Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Flexible SL60 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 166 - 182 °C | 331 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable WR3792CL Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 193 °C | 331 - 379 °F | Blown Film |
Chevron Phillips K-Resin® KR10 Styrene-Butadiene Copolymer, Film Grade
(discontinued **) Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: This SBC is easily processed on blown film or cast fi.. |
|||
Melt Temperature | 166 - 182 °C | 331 - 360 °F | Extrusion |
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l.. |
|||
Melt Temperature | 166 - 193 °C | 331 - 379 °F | Blown Film |
Chevron Phillips K-Resin® DK11 Styrene-Butadiene Copolymer, Film Grade Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: Provides the same high performance film properties as.. |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable 1721-xx14E Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 193 °C | 331 - 379 °F | Blown Film |
Chevron Phillips K-Resin® DK13 Styrene-Butadiene Copolymer, Film Grade
(discontinued **) Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: DK13 is an SBC designed for the film market and has i.. |