Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 140 - 280 °C | 284 - 536 °F | Average value: 197 °C Grade Count:347 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Melt Temperature | 140 - 180 °C | 284 - 356 °F | Injection Molding |
Stellarchem MP-835B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Melt Temperature | 140 - 180 °C | 284 - 356 °F | |
Borealis FA7224 Low Density Polyethylene FA7224 has been developed for applications such as: Thin bags with excellent optical and slip properties, and laundry and other textile bags. Contains antioxidant.Information provided by Borealis AG.. |
|||
Melt Temperature | 140 - 180 °C | 284 - 356 °F | |
Borealis FA7229 Low Density Polyethylene FA7229 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant and Cling additive. Applications: food wrap film, lamination films, blending, and other blown cling film.Information pr.. |
|||
Melt Temperature | 140 - 180 °C | 284 - 356 °F | |
Borealis LE0563 Polyethylene Compound, Thermoplastic, Semiconductive LE0563 is a thermoplastic semi conductive compound specifically designed for medium- and high voltage cable systems requiring improved grounding. It may be used either as a complete jacket or as a t.. |
|||
Melt Temperature | 140 - 200 °C | 284 - 392 °F | Average value: 173 °C Grade Count:22 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |
|||
Melt Temperature | 140 - 190 °C | 284 - 374 °F | |
Polyplastic TechnoTep A® 65 A Thermoplastic Elastomer, Mineral Filled Low mineral filled, good flexibilityInformation provided by PolyPlastic Group. |