Processing Properties Metric English Comments
Melt Temperature 125 - 130 °C
257 - 266 °F
Polyplastic Torlen® PE 2K 901 High Density Polyethylene, Carbon Filled
Information provided by PolyPlastic Group.
Melt Temperature 125 - 232 °C
257 - 450 °F
Average value: 190 °C Grade Count:18
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..
Melt Temperature 125 °C
257 °F
A. Schulman CP80-01 Linear Low-Density Polyethylene
DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In..
Melt Temperature 125 °C
257 °F
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In..
Melt Temperature <= 125 °C
<= 257 °F
Borealis FR4830 Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires
FR4830 is a chemically crosslinkable Non-halogen flame retardant Polyethylene compound for Primary Automotive and Appliance Wire. Applications: FR4830 is intended for use as a 125º C rated primary ..
Melt Temperature 125 - 130 °C
257 - 266 °F
Borealis Supercure™ LC8205R Polyethylene Insulation Compound, Crosslinkable
Supercure™ LC8205R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: Supercure™ LC8205R is intended for insulation of XLPE power cabl..
Melt Temperature 125 °C
257 °F
A. Schulman CP80-01 Linear Low-Density Polyethylene
DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In..
Melt Temperature 125 - 175 °C
257 - 347 °F
blown film extrusion
DuPont Elvax® 3170 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.Elvax® 3170 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins..
Melt Temperature 125 - 175 °C
257 - 347 °F
blown film extrusion
DuPont Elvax® 3170SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.Elvax® 3170SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res..
Melt Temperature 125 °C
257 °F
A. Schulman CP80-01 Linear Low-Density Polyethylene
DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In..
Melt Temperature 125 °C
257 °F
A. Schulman CP80-01 Linear Low-Density Polyethylene
DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In..
Melt Temperature 125 °C
257 °F
A. Schulman CP80-01 Linear Low-Density Polyethylene
DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In..
Melt Temperature 125 °C
257 °F
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In..
Melt Temperature 125 °C
257 °F
A. Schulman CP80-01 Linear Low-Density Polyethylene
DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In..
Melt Temperature 125 °C
257 °F
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In..
Melt Temperature 125 °C
257 °F
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In..
Melt Temperature 125 °C
257 °F
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In..
Melt Temperature 125 °C
257 °F
A. Schulman CP878-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 878-01 Natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties. ApplicationCP 878-01 meets FDA Regulation 21 CFR 177.1520(c)3.1 and 3.2.In..
Melt Temperature 125 - 185 °C
257 - 365 °F
Borealis LE7704 Polyethylene Compound, Semiconductive, Thermoplastic
LE7704 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7704 is intended for semiconductive applications in medium voltage..