Material Notes:
LE7704 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7704 is intended for semiconductive applications in medium voltage cables. Specifications: IEC 60502 ISO 1872-E/BA, KHXY, 23-G200, C40Information provided by Borealis AG
Physical Properties Metric English Comments
Density 1.135 g/cc
0.04100 lb/in³
ISO 1183/ISO 1872-2
Water Absorption 0.060 %
0.060 %
Karl Fischer-titration
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 2.20 MPa
<= 319 psi
after aging (168h, 135°C); IEC 60811-1-2
11.0 MPa
1600 psi
25mm/min; ISO 527
Elongation at Break 200 %
200 %
25mm/min; ISO 527
Electrical Properties Metric English Comments
Volume Resistivity <= 100 ohm-cm

@Temperature 23.0 °C
<= 100 ohm-cm

@Temperature 73.4 °F
DC; ISO 3915
<= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
DC; ISO 3915
Processing Properties Metric English Comments
Processing Temperature 60.0 °C
140 °F
hopper drying; 4h
Melt Temperature 125 - 185 °C
257 - 365 °F
Shelf Life 12.0 Month
12.0 Month