Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 31 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress, UL listed molding compound 1.5 mm/V-1 (All), 3 mm/V-0 (All), standardized molding compound.Applicat.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 31.5 Phenolic Formaldehyde Resin, Improved Electrical Properties
(discontinued **) Phenolic molding compound, mainly organically filled, electrically high grade, standardized molding compound.Application areas: Parts for electrical and telecommunications technology, car electronic.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 31.9 Phenolic Formaldehyde Resin, Ammonia Free
(discontinued **) Phenolic molding compound, mainly organically filled, ammonia free, standardized molding compound.Application areas: Parts for electrical and telecommunications technology, motor vehicle ignition sy.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 51 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, switch.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 85 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, average notched impact strength, UL listed molding compound 1.5 mm/HB (BK, BN).Application areas: Switch covers, rolls, .. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 1107 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures
(disconti Phenolic molding compound, inorganically filled, glass fiber reinforced, high heat resistance, low heat expansion coefficient, highest resistance to pressure, high dimensional stability.Application .. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, hot steam and hot water resistant (not suitable for use of higher voltage).Application.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 2137 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof
(discontinued ** Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, minimal distortion, dish washer proof.Application areas: Iron heat shields, fittings f.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 2535 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof
(discontinued ** Phenolic molding compound, inorganically/organically filled, average heat resistant, steam resistant, dish washer proof, high surface quality.Application areas: Fittings for ovens and dishwashers, t.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 2774 Phenolic Formaldehyde Resin, Dishwasher Proof, Improved Electrical Properties, Low Shrinkage, UL Listed Phenolic molding compound, inorganically filled, glass fiber reinforced, increased dimensional stability, averaged notched impact strength, average heat resistance, improved electrical properties, U.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 6506 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures, UL Listed
&nbs Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant, UL listed molding compound 1.5 mm/V-.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 6507 Phenolic Formaldehyde Resin, Elasticized, Low Shrinkage, Resistant to High Temperatures, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, elastomer modified, galvanizable, heat resistant, good media resistance, high dimensional stability at raised temperature, hi.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 7400 Phenolic Formaldehyde Resin, High Mechanical Strength
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fiber flakes, high notched impact strength.Application areas: Moldings for higher mechanical strain, e.g. power plugs high volta.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 14600 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled, low specific gravity.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a part of Hexion in 2005.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 14694 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds.Application areas: Housing parts, heat shields, cookware fittings.Information provided by Bak AGBak AG became a p.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 38110 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled.Application areas: Devices for the electrical installation, pan handles, knobs, mainly for compression molding.Information provided by Bak AGBak .. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ 151733 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Contact strips.Information provided by Bak AGBak AG became a part of Hexion in 20.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ 460124 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ X22 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Pot handles, operating controls, electrical isolators, housing parts.Informati.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ X30 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, reinforced with cotton and sisal fibers, increased notched impact strength.Application areas: Covers for electrical and electromagnetic devices.Information provided by Bak.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 7595 Phenolic Formaldehyde Resin, Low Coefficient of Friction, Galvanized, Conductive
(di Phenolic molding compound, inorganically/organically filled, modified with graphite, good heat conductivity, good sliding properties, conductive in electrical properties.Application areas: Bearers f.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled. Excellent heat resistance with respect to surface finish and mechanical properties.Application areas: Pan handles, heat r.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 83 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Switch covers, rolls, handle casings.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 4155 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, good media and temperature resistance. Conditioned Cu-adhesion.Application areas: Commutators (fuel pumps, actuators, starte.. |
|||
Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
Hexion Bakelite™ PF 4260 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistantApplication areas: Commutators (starte.. |