Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 271 - 299 °C | 520 - 570 °F | |
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled PC/ABS Alloy, General Purpose, 10% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1013THL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1013THL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 271 - 299 °C | 520 - 570 °F | |
Polymer Resources PC/ABS-G30 General Purpose PC/ABS Alloy, 30% Glass Filled PC/ABS Alloy, General Purpose, 30% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Melt Temperature | 271 - 299 °C | 520 - 570 °F | |
Polymer Resources PC/ABS-G40 General Purpose PC/ABS Alloy, 40% Glass Filled PC/ABS Alloy, General Purpose, 40% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1033L Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1033L Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1033TL Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |