Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 30.0 - 60.0 min @Temperature 60.0 °C |
30.0 - 60.0 min @Temperature 140 °F |
|
Abatron AboCast/AboCure 8109-13 Liquid hardener version of AboCast/AboCure 8109-11.Processing: 100/23 pbw; Potlife: 3-5 h/20°C (68°F), 1-3 h/40°C (105°F), 0.5-1 h/60°C (140°F); mix at RT; cures in: 30 mins/60°C (140°F), 45.. |
|||
Pot Life | 30.0 min @Temperature 40.0 °C |
30.0 min @Temperature 104 °F |
|
Abatron AboCast/AboCure 8109-3 Low viscosity, RT cure. Easy processing.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140.. |
|||
Pot Life | 30.0 min @Temperature 40.0 °C |
30.0 min @Temperature 104 °F |
|
Abatron AboCast/AboCure 8109-4 Safety hardener (minimum toxicity) version of 8109-3.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 .. |