Processing Properties | Metric | English | Comments |
---|---|---|---|
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200H-20 Polyester SMC Premi-Glas® 1200H-20 is a 20% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94HB flame rec.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200H-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1201-15 Polyester SMC Premi-Glas® 1201-15 is a 15% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1203-30 Fiberglass Reinforced SMC Description: Premi-Glas® 1203-30 is a fiberglass-reinforced, thermoset sheet molding compound designed for structural and semi-structural components where smooth flat surfaces, high strength and st.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1205 Glass Reinforced SMC Description: Premi-Glas® 1205 is a glass reinforced thermoset Sheet Molding Compound formulated for residential door skins and similar construction applications. Key features and benefits: Excellen.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1206 LD Fiberglass Reinforced Thermoset SMC Premi-Glas® 1206 LD is a fiberglass reinforced thermoset sheet molding compound for transportation or structural and semi-structural applications where good surface appearance, high strength and du.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2103-25 CRSX Polyester BMC Premi-Glas® 2103-25 CR-SX is a 25% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2143-24 CR-SX Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2143-24 CR-SX-HT Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2200-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2200-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Pigmentable for molded-in c.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2200-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2203-15 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-15 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2203-20 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-20 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2203-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2203-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2204-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2204-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2204-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2550® CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas 2550® CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generation .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3101-20 Polyester BMC Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL 94-.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3101-22 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-22 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3200-15 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-15 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3200-20 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-20 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3200-30 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-30 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3404 33% Glass Reinforced SMC Description: Premi-Glas® 3404 is a glass reinforced thermoset sheet molding compound designed for mass transit and high strength flame retardant applications where low smoke and flame are required... |
|||
Clamp Pressure | 2.07 - 6.89 MPa | 300 - 1000 psi | |
Quantum Composites AMC™ 8595 55% Carbon Fiber Reinforced Vinyl Ester SMC AMC™ 8595 is a vinyl ester engineered structural composite molding compound with continuous, unidirectional carbon fibers. It is designed for compression molding of components requiring high struc.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1281-47 VE SMC Description: Premi-Glas® 1281-47 VE is a sheet molding compound.Market: StructuralInformation provided by Premix. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2103-15 CRSX Polyester BMC Premi-Glas® 2103-15 CR-SX is a 15% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |