Processing Properties | Metric | English | Comments |
---|---|---|---|
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1100-20 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-20 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1100-25 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1100V-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-10 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200-30 Polyester SMC Premi-Glas® 1200-30 is a fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck and Marine body panels and interior structural components where smooth flat surfac.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200H-15 Polyester SMC Premi-Glas® 1200H-15 is a 15% fiberglass-reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94 HB flame re.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1200H-30 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-30 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1201-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1201-20 is a fiberglass reinforced thermoset sheet molding compound for sanitary ware applications such as shower bases and surrounds, bathtubs and vanity tops.Key features and benefits.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1203-30 Fiberglass Reinforced SMC Description: Premi-Glas® 1203-30 is a fiberglass-reinforced, thermoset sheet molding compound designed for structural and semi-structural components where smooth flat surfaces, high strength and st.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1240-15 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-15 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1240-20 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-20 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1240-25 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-25 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2200-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2200-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2204-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2204-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2204-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2205-20 CRSX Polyester SMC Premi-Glas® 2205-20 CR-SX is a 20% fiberglass reinforced Sheet Molding Compound formulated for condensate pan applications requiring chemical resistance, heat resistance, dimensional stability, we.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2205-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2205-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-15 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2206-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 2207-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3101-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-15 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3101-20 Polyester BMC Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL 94-.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3101-22 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-22 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3200-15 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-15 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Clamp Pressure | 3.45 - 6.89 MPa | 500 - 1000 psi | Molding Pressure |
Premix Premi-Glas® 1286 Glass Reinforced SMC Description: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression molding.. |