Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Cure Time = 0.667 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 20.0 - 40.0 min
0.333 - 0.667 hour
On steel (Fixture)
ND Industries 541 Shaft & Bearing Retainer Retaining Compound
Very high strength retainer for gears, wheels, pulleys, cams, collars, flywheels, rotors to shaft
Cure Time 20.0 - 40.0 min
0.333 - 0.667 hour
On steel (Fixture)
ND Industries 542 Shaft & Bearing Retainer Retaining Compound
Very high strength retainer for gears, wheels, pulleys, fans, cams, collars, flywheels, rotors to shaftMeets military spec Mil-R-46082B Type III
Cure Time 20.0 - 40.0 min
0.333 - 0.667 hour
working strength
Permabond TA439 Toughened Acrylic Adhesive
Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f..
Cure Time 30.0 - 40.0 min

@Temperature 25.0 °C
0.500 - 0.667 hour

@Temperature 77.0 °F
Handling strength
Lord Adhesives Versilok® 253 / 254 Acrylic Adhesive
LORD Versilok® 253/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum..
Cure Time 30.0 - 40.0 min

@Temperature 25.0 °C
0.500 - 0.667 hour

@Temperature 77.0 °F
Handling strength
Lord Adhesives Versilok® 262 / 254 Acrylic Adhesive
LORD Versilok® 262/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi..
Cure Time 30.0 - 40.0 min
0.500 - 0.667 hour
Working time
ITW Devcon Safety Clear Coatâ„¢ Epoxy, Water Clear
Information provided by ITW Devcon
Cure Time 20.0 - 40.0 min
0.333 - 0.667 hour
Setting Time
Chosun Refractories APC-1 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 20.0 - 40.0 min
0.333 - 0.667 hour
Setting Time
Chosun Refractories APC-2 Special Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved