Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6008 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6013 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6014 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6101 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6103 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6201 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6206 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6502 Adhesive Description: The CYNERGY 6500 SERIES are black, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6809 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6902 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Cure Time | 480 min | 8.00 hour | Full Cure |
Resinlab® RC8038 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6802 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6803 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 480 min | 8.00 hour | Full cure |
Resinlab® CYNERGY CA6806 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 480 min | 8.00 hour | |
Lord Adhesives 370 Two Component Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Cure Time | 480 - 600 min | 8.00 - 10.0 hour | Functional cure |
ITW Devcon Safety Clear Coatâ„¢ Epoxy, Water Clear Information provided by ITW Devcon |
|||
Cure Time | 480 min | 8.00 hour | 4 hrs @ 25°C + 4 hrs @ 65°C-plus |
Tra-Con Tra-Bond 2114 Water White Transparent Epoxy Adhesive TRA-BOND 2114 is a transparent, low viscosity epoxy resin formulation recommended for industrial adhesive and laminating applications where sparkling clarity and excellent structural, mechanical and.. |
|||
Cure Time | 480 min | 8.00 hour | 4 hrs @ 25°C + 4 hrs @ 65°C |
Tra-Con Tra-Bond 2110 High Impact Epoxy Staking Compound TRA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, n.. |
|||
Cure Time | 480 min | 8.00 hour | 4 hrs @ 25°C + 4 hrs @ 65°C |
Tra-Con Tra-Bond 2125 Rigid Syntactic Repair Adhesive TRA-BOND 2125 is a medium viscosity, low density syntactic foam epoxy formulation developed for industrial, electronic and aerospace honeycomb, fillet, edge-fill, contour repair, bonding and casting.. |
|||
Cure Time | 480 min | 8.00 hour | Tack-Free Time |
3M AC-251 Black Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-251 Black Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate ai.. |
|||
Cure Time | 480 min | 8.00 hour | Hard Dry |
3M Scotchkote™ LW 405 Epoxy Concrete Mortar Scotchkote Epoxy Concrete Mortar LW 405 has been specifically developed as a three component 100% solids light weight repair mortar for use on concrete surfaces.Product Features:Designed for applica.. |
|||
Cure Time | 480 min | 8.00 hour | Hard Dry |
3M Scotchkote™ RS 820 Epoxy Screed Scotchkote Epoxy Sceed RS 820 has been specially developed as a three component 100% solids resurfacing screed for application to concrete floor surfacesProduct Features:Combines good application ch.. |
|||
Cure Time | 480 min | 8.00 hour | |
3M Scotch-Weld™ 1838L B/A Two-Part Structural Adhesive Multi-purpose and Rigid bondsInformation provided by 3M |
|||
Cure Time | 480 - 720 min @Temperature 24.0 °C |
8.00 - 12.0 hour @Temperature 75.2 °F |
|
BCC Products BC 5008-2 General Purpose Epoxy System BC 5008-2 is a very low viscosity, modified, unfilled, room temperature curing, general purpose resin system. BC 5008-2 is a clear, amber, medium pot life material, with heat resistance to 175ºF. A.. |
|||
Cure Time | 480 - 720 min @Temperature 24.0 °C |
8.00 - 12.0 hour @Temperature 75.2 °F |
demold time |
BCC Products DP-11-88 Urethane Adhesive DP-11-88 is a medium viscosity quick setting easy to use urethane adhesive. This system was specifically designed to bond together the MB2001/MB3000 Model/Tooling Board to create desired dimensions .. |
|||
Cure Time | 480 min | 8.00 hour | Full Cure |
Resinlab® RC8009 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Cure Time | 480 min | 8.00 hour | Full Cure |
Resinlab® RC8080 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Cure Time | 480 - 720 min @Temperature 24.0 °C |
8.00 - 12.0 hour @Temperature 75.2 °F |
|
BCC Products BC 5010 Epoxy Laminating System BC 5010 is a high quality, low viscosity room temperature curing laminating resin. A Safety System for the production of a variety of dimensionally stable fiberglass tools. BC 5010 features low odor.. |