Material Notes:
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products form a tough permanent bond which greatly enhances the torque and pullout strength. They are single component solvent free materials manufactured in a wide variety of viscosities and setting times to satisfy specific bonding applications. This technology increases the reliability and performance of assemblies while reducing dependence upon maintaining costly tight machining tolerances.Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Viscosity 125 cP
125 cP
Mechanical Properties Metric English Comments
Shear Strength 26.2 MPa
3800 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 350 °C
662 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Processing Properties Metric English Comments
Cure Time 15.0 min
0.250 hour
Fixture
480 min
8.00 hour
Full Cure
Descriptive Properties Value Comments
Color Green
Gap Fill (mil) 5