Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 1800 min @Temperature 170 °C |
30.0 hour @Temperature 338 °F |
|
Humiseal 1A27 Urethane Conformal Coating Humiseal 1A27 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedPasses thermal shock test (MIL-I-46058C)Flammabilit.. |
|||
Cure Time | 1800 min @Temperature 170 °C |
30.0 hour @Temperature 338 °F |
|
Humiseal 1A27LSE Urethane Conformal Coating Humiseal 1A27LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingPasses thermal shock test (MIL-I-46058C).. |
|||
Cure Time | 1800 min @Temperature 170 °C |
30.0 hour @Temperature 338 °F |
|
Humiseal 1A33 Urethane Conformal Coating Humiseal 1A33 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL.. |
|||
Cure Time | 1800 min @Temperature 170 °C |
30.0 hour @Temperature 338 °F |
|
Humiseal 1A33LSE Urethane Conformal Coating Humiseal 1A33LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses ther.. |
|||
Cure Time | 1800 min | 30.0 hour | Cover mold with polyethylene sheet or locate in a humidity chamber for 24 hrs; 3 hrs at 200°F; 3 hrs at 250°F |
Aremco Ceramacast™ 510 High Temperature Potting & Casting Material Alumina Coarse grain castable for producing large hi-temp tooling. |
|||
Cure Time | 1800 min | 30.0 hour | Tack-Free Time |
3M AC-240 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |
|||
Cure Time | 1800 min | 30.0 hour | |
3M AC-240 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |