Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 720 min | 12.0 hour | On steel (Full) |
ND Industries 732 Gasket Maker Flexible Flexible Parts. General Purpose |
|||
Cure Time | 720 - 1440 min | 12.0 - 24.0 hour | Full cure for handling |
P & P Technology MS-N Nickel Graphite Conductive Adhesive P & P Technology conductive nickel/graphite adhesive is a one part electrically conductive room temperature curing elastomer. It is supplied as a readily extrudable paste that cures rapidly when exp.. |
|||
Cure Time | 720 - 1440 min | 12.0 - 24.0 hour | Cure for Handling |
P & P Technology Silver/Aluminum Conductive Adhesive P & P Technology conductive silver/aluminum adhesive is a one part electrically conductive room temperature curing elastomer. It is supplied as a readily extrudable paste that cures rapidly when exp.. |
|||
Cure Time | 720 min @Temperature 25.0 °C |
12.0 hour @Temperature 77.0 °F |
Thin Film Set |
Protective Coating PC-Rot Terminator® Epoxy Wood Consolidant Description: PC-Rot Terminator® is designed to strengthen decayed or rotted wood. The mixture is a low viscosity liquid that penetrates porous surfaces filling and sealing voids with an epoxy that .. |
|||
Cure Time | 720 min | 12.0 hour | Ambient, tack free |
Reltek BONDiT™ B-45 Adhesive, Sealant & Coating System Key Properties: Excellent adhesive for low surface energy plastics without primer.Used in potting, painting and protective coating applications.Excellent thermal and mechanical shock resistance.Ease.. |
|||
Cure Time | 720 min | 12.0 hour | Ambient, tack free |
Reltek BONDiT™ B-45TH Adhesive, Sealant & Coating System Key Properties: Excellent adhesion to low surface energy plastics without primer.Bonding dissimilar materials.Chemical and shock resistance.Ease of use.Applications: Bonds difficult-to-bond substrat.. |
|||
Cure Time | 720 min | 12.0 hour | Ambient, tack free |
Reltek BONDiT™ B-482 Adhesive, Sealant & Coating System Key Properties: Excellent balance of chemical, electrical, and mechanical properties.Ruggedized, semi-flexible system.Very clean system.Ease of use.Applications: Encapsule sensitive instrumentation .. |
|||
Cure Time | 720 min | 12.0 hour | Ambient, tack free |
Reltek BONDiT™ B-481 Adhesive, Sealant & Coating System Key Properties: High strength and toughness with excellent thermal stability to 400°F.Outstanding chemical resistance.Excellent electrical, and mechanical properties.Ease of use.Applications: Encap.. |
|||
Cure Time | 720 min | 12.0 hour | Functional cure |
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Putty, Black Information provided by ITW Devcon |
|||
Cure Time | 720 min | 12.0 hour | Functional cure |
ITW Devcon Flexane® Rubber Repair / Castable Urethane Belt Repair Kit, Black Information provided by ITW Devcon |
|||
Cure Time | 720 min | 12.0 hour | Through |
Momentive Performance Materials RTV5812 One-Component, Modified Alkoxy Adhesive Sealant, White RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Cure Time | 720 min | 12.0 hour | Through |
Momentive Performance Materials RTV5813 One-Component, Modified Alkoxy Adhesive Sealant, Black RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Cure Time | 720 min | 12.0 hour | Through |
Momentive Performance Materials RTV5818 One-Component, Modified Alkoxy Adhesive Sealant, Translucent RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Cure Time | 720 - 1440 min @Temperature 23.0 °C |
12.0 - 24.0 hour @Temperature 73.4 °F |
|
Master Bond Mastersil 410 One Component Room Temperature Curing Silicon Master Bond MasterSil 410 is a ready-to-use, one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. This compound has a pas.. |
|||
Cure Time | 720 - 1440 min @Temperature 23.0 °C |
12.0 - 24.0 hour @Temperature 73.4 °F |
|
Master Bond Mastersil 415 One Component Room Temperature Curing, Transparent Silicon Master Bond MasterSil 415 is a ready-to-use, one component high performance silicone elastomer compound for bonding, sealing and protective coatings featuring high transparency. It has a paste consi.. |
|||
Cure Time | 720 - 1440 min @Temperature 23.9 °C |
12.0 - 24.0 hour @Temperature 75.0 °F |
|
Master Bond X17MED Elastomer Compound for Medical Device Applications Description: Master Bond Polymer System X17MED is a specially formulated one component adhesive specially designed for bonding polyolefins such as polypropylene and polyethylene as well as their man.. |
|||
Cure Time | 720 min | 12.0 hour | 2 hrs @ 25°C + 10 hrs @ 55°C |
Tra-Con Tra-Cast 3010 Flexible Clear Epoxy Casting Compound TRA-CAST 3010 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties, good clarity, long pot life.. |
|||
Cure Time | 720 - 960 min | 12.0 - 16.0 hour | |
Trelleborg Emerson & Cuming Stycast® 1497 Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Cure Time | 720 min @Temperature 25.0 °C |
12.0 hour @Temperature 77.0 °F |
|
Epoxyset Epoxibond EB-103F Unfilled Epoxy Adhesive A two-component, unfilled, fast setting epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries. EB-103F has excellent bond strength to v.. |
|||
Cure Time | >= 720 min @Temperature 22.0 - 30.0 °C |
>= 12.0 hour @Temperature 71.6 - 86.0 °F |
|
Abatron AboCoat 8709-7 Nickel-Filled Electrically Conductive Acrylic Compound AboCoat 8709-7 is an easy-to-use nickel-acrylic conductive coating. |
|||
Cure Time | 720 min | 12.0 hour | |
3M AC-350 Class A-2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have.. |
|||
Cure Time | 720 min | 12.0 hour | |
3M AC-665 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-665 Class B are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros.. |
|||
Cure Time | 720 min | 12.0 hour | Tack-Free Time |
3M AC-736 B-2 Aerospace Sealant 3M Aerospace Sealant AC-736 B-2 is a non-chromate corrosion inhabiting sealants, fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealant. These Sealants act as an .. |
|||
Cure Time | 720 min | 12.0 hour | |
3M AC-736 B-2 Aerospace Sealant 3M Aerospace Sealant AC-736 B-2 is a non-chromate corrosion inhabiting sealants, fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealant. These Sealants act as an .. |
|||
Cure Time | 720 min | 12.0 hour | Touch Dry |
3M Scotchkote™ 152LV Epoxy Coating Scotchkote Epoxy Coating 152LV has been specifically developed as a surface tolerant anti corrosive coating for steel structures.Product Features:Combines good application characteristics with excel.. |
|||
Cure Time | 720 - 1080 min @Temperature 24.0 °C |
12.0 - 18.0 hour @Temperature 75.2 °F |
|
BCC Products BC 7062H Epoxy Casting BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi.. |
|||
Cure Time | 720 - 960 min | 12.0 - 16.0 hour | Time to Handling Strength |
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |