Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 30.0 min | 0.500 hour | With Primer (Fixture) |
ND Industries 440 High pressure Sealant Pneumatic and hydraulic sealant fluid, for power and gas system connections |
|||
Cure Time | 30.0 min @Temperature 150 °C |
0.500 hour @Temperature 302 °F |
Oven |
Permabond ES550 Epoxy Resin PERMABOND ES550 is a single-part epoxy paste which is slump-resistant (does not flow) during cure. The adhesive is toughened for maximum impact resistance, along with excellent peel and shear streng.. |
|||
Cure Time | 30.0 min @Temperature 150 °C |
0.500 hour @Temperature 302 °F |
Oven |
Permabond ES578 Epoxy Resin PERMABOND® ES578 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces, ceramics as well as composite materials. ES578 provides excellent thermal conductivity and bon.. |
|||
Cure Time | 30.0 min @Temperature -55.0 - 150 °C |
0.500 hour @Temperature -67.0 - 302 °F |
Handling |
Palm Labs Adhesives TURBO-LOCK SERIES 15 Anaerobic Thread Locking Compound TURBO-LOCK 15 SERIES is a fast curing, large bolt, RED, high strength, anaerobic thread-locking compound for bonding and sealing threads. Prevents rusting of threads. It is highly resistance to heat.. |
|||
Cure Time | 30.0 min @Temperature 152 °C |
0.500 hour @Temperature 305 °F |
|
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Cure Time | 30.0 min @Temperature 142 °C |
0.500 hour @Temperature 287 °F |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 66A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Cure Time | 30.0 min @Temperature 210 °C |
0.500 hour @Temperature 410 °F |
|
Lord Adhesives 8621 Polymer Resistor Composition LORD 8600 series polymer resistor compositions are designed for screen print application onto a wide range of substrates.All information provided by Lord. |
|||
Cure Time | 30.0 min @Temperature 150 °C |
0.500 hour @Temperature 302 °F |
|
Lord Adhesives Thermosetâ„¢ ME-455 Epoxy Board Level Encapsulant LORD Thermosetâ„¢ ME-455 encapsulant is a onecomponent, semiconductor grade epoxy designed for the encapsulation of wire-bonded or flip chip die in PPGA, BGA, MCM and other cavity packages. It is.. |
|||
Cure Time | 30.0 - 35.0 min | 0.500 - 0.583 hour | Fixture time |
ITW Devcon 2 Ton® Epoxy Clear Epoxy, Clear, White Information provided by ITW Devcon |
|||
Cure Time | 30.0 min @Temperature 120 °C |
0.500 hour @Temperature 248 °F |
|
Tra-Con Tra-Duct 921H01 Information provided by Tra-Con Inc. |
|||
Cure Time | >= 30.0 min | >= 0.500 hour | |
Trelleborg Emerson & Cuming Stycast® XT-5038-9 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Cure Time | 30.0 min | 0.500 hour | |
Loctite® 272 High Temperature/High Strength Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Cure Time | 30.0 min @Temperature 152 °C |
0.500 hour @Temperature 305 °F |
|
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 60 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Cure Time | 30.0 - 60.0 min | 0.500 - 1.00 hour | |
Trelleborg Emerson & Cuming Stycast® 2850FT-FR/11 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Cure Time | 30.0 - 240 min | 0.500 - 4.00 hour | Full Cure; Primed |
Loctite® Gasket Eliminator® 518 Flange Sealant Anaerobic GasketingLoctite® 518 Flexible Cure Gasket Eliminator® Flange SealantForms a flexible, solvent-resistance seal that will not tear or decay. Seals to 300ºF and fills gaps to 0.050". Can.. |
|||
Cure Time | 30.0 min @Temperature 180 °C |
0.500 hour @Temperature 356 °F |
|
Dow BETAMATE™ 1045 Epoxy BETAMATE™ 1045 is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excellent.. |
|||
Cure Time | >= 30.0 min @Temperature 75.0 °C |
>= 0.500 hour @Temperature 167 °F |
tack free |
ACC EP RAP-1567 HX EPI Engineered Polymers Aliphatic Polyurea RAP-1567 is a two component 100% solids, no VOC’s, aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generation.. |
|||
Cure Time | >= 30.0 min @Temperature 75.0 °C |
>= 0.500 hour @Temperature 167 °F |
tack free |
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea RAP-1567 SP is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This ne.. |
|||
Cure Time | 30.0 min @Temperature 25.0 °C |
0.500 hour @Temperature 77.0 °F |
Cooling time |
Aquabond Technologies Aquabond™ ABS-55 Water Soluble Adhesive and Bonding Thermoplastic Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem.. |
|||
Cure Time | 30.0 - 60.0 min | 0.500 - 1.00 hour | Air Set prior to curing |
Aremco Aremco-Seal™ 529 High Temperature Specialty Coatings Silicone Transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Cure Time | 30.0 min | 0.500 hour | Pressing Time |
3M 5010 Polyurethane Multi-Purpose Adhesive 3M™ Polyurethane Multi-Purpose Adhesive 5010 is a one component, fast curing adhesive which forms a rigid permanent bond. 3M 5010 bonds to a wide variety of materials including wood, foam panels, f.. |
|||
Cure Time | >= 30.0 min @Temperature 75.0 °C |
>= 0.500 hour @Temperature 167 °F |
tack free |
ACC EP RAP 45 14 EPI Engineered Polymers Aliphatic Polyurea EP RAP 45 14 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC’s, aliphatic polyurea coating that was developed for UV stable (colorfast) polyurea f.. |
|||
Cure Time | 30.0 - 240 min | 0.500 - 4.00 hour | Full Cure; Primed |
Loctite® Gasket Eliminator® 510 Flange Sealant Anaerobic GasketingLoctite® 510 High Temperature Rigid Cure Gasket Eliminator® Flange SealantProduct has a temperature range to 400ºF with excellent solvent and chemical resistance. Makes or dre.. |